References from Target polishing of KDP crystals by organic acid-ionic liquid-in-oil microemulsions. Local targets link to admitted publications; unresolved targets remain external evidence.
Developing KH2PO4 and KD2PO4 crystals for the world's most power laser
10.1179/095066001225001085 · 2002 · External reference
Large Optics for the national ignition facility
10.13182/fst15-143 · 2016 · External reference
Design and development of pockels cell driver for Q switch LASER in space applications
10.1080/03772063.2017.1322925 · 2017 · External reference
Characteristics of nonlinear optical absorption and refraction for KDP and DKDP crystals
10.1364/ome.7.000533 · 2017 · External reference
NIF optical materials and fabrication technologies: an overview
2004 · External reference
Research of target uniform illumination on SG-III laser facility
2016 · External reference
Research on the low speed stability control technology of Fly-cutting machine tool for KDP crystals
2014 · External reference
Fine diamond turning of KDP crystals
10.1364/ao.25.001733 · 1986 · External reference
Characterization of KDP crystal surfaces from single point diamond milling
10.4028/www.scientific.net/amr.1136.271 · 2016 · External reference
Laser-induced damage of KDP crystals by 1 omega nanosecond pulses: influence of crystal orientation
10.1364/oe.17.021652 · 2009 · External reference
Understanding the formation mechanism of subsurface damage in potassium dihydrogen phosphate crystals during ultra-precision fly cutting
10.1007/s40436-019-00265-2 · 2019 · External reference
Formation and suppression of KDP surface defects generated in fly-cutting process
2018 · External reference
Magnetorheological finishing (MRF) of potassium dihydrogen phosphate (KDP) crystals: nonaqueous fluids development, optical finish, and laser damage performance at 1064 nm and 532 nm
2009 · External reference
Effects of temperature on the removal efficiency of KDP crystal during the process of magnetorheological water-dissolution polishing
10.1364/ao.55.008308 · 2016 · External reference
Preparation of methoxyl poly(ethylene glycol) (MPEG)-coated carbonyl iron particles (CIPs) and their application in potassium dihydrogen phosphate (KDP) magnetorheological finishing (MRF)
10.1016/j.apsusc.2015.06.063 · 2015 · External reference
Novel magnetorheological figuring of KDP crystal
2011 · External reference
Research of polishing process to control the iron contamination on the magnetorheological finished KDP crystal surface
10.1364/ao.54.001478 · 2015 · External reference
Optimization of morphological parameters for mitigation pits on rear KDP surface: experiments and numerical modeling
10.1364/oe.25.018332 · 2017 · External reference
The magnetorheological finishing (MRF) of potassium dihydrogen phosphate (KDP) crystal with Fe3O4 nanoparticles
10.1186/s11671-016-1301-4 · 2016 · External reference
Study on the feasibility of ion beam figuring on DKDP crystal
2017 · External reference
Figuring process of potassium dihydrogen phosphate crystal using ion beam figuring technology
10.1364/ao.56.007130 · 2017 · External reference
Research on temperature field of KDP crystal under ion beam cleaning
10.1364/ao.55.004888 · 2016 · External reference
Process optimization in optical fabrication
10.1117/1.oe.55.3.035106 · 2016 · External reference
A review on recent advances in machining methods based on abrasive jet polishing (AJP)
10.1007/s00170-016-9405-7 · 2017 · External reference
A novel multi jet polishing process and tool for high-efficiency polishing
10.1016/j.ijmachtools.2016.12.006 · 2017 · External reference
Mitigation of subsurface damage in potassium dihydrogen phosphate (KDP) crystals with a novel abrasive-free jet process
10.1364/ome.8.002625 · 2018 · External reference
Theoretical modeling and analysis of material removal characteristics for KDP crystal in abrasive-free jet processing
10.1364/oe.27.006268 · 2019 · External reference
Experimental study on micro-deliquescence ultra-precision polishing with fine water mist for KDP crystal
2013 · External reference
Research on deliquescent polishing fluid for KDP crystals
2009 · External reference
Water-in-Oil dispersion for KH2PO4 (KDP) crystal CMP
10.1080/01932690903297330 · 2010 · External reference
KDP aqueous solution-in-oil microemulsion for ultra-precision chemical-mechanical polishing of KDP crystal
10.3390/ma10030271 · 2017 · External reference
Novel abrasive-free jet polishing mechanism for potassium dihydrogen phosphate (KDP) crystal
10.1364/ome.8.001012 · 2018 · External reference
Residual stress fields analysis in rolled Zircaloy-4 plates: grazing incidence diffraction and elastoplastic self-consistent model
10.1016/j.actamat.2014.02.031 · 2014 · External reference
Equi-penetration grazing incidence X-ray diffraction method: stress depth profiling of ground silicon nitride
10.1016/j.actamat.2014.06.015 · 2014 · External reference
Unresolved reference
1977 · External reference
The Raman effect in crystals
10.1080/00018730110101395 · 2001 · External reference
Phase transitions and amorphization in KD2PO4 and KH2PO4 under high pressure
10.1103/physrevb.65.132105 · 2002 · External reference
Phase transitions and amorphization of KH2PO4 at high pressure
10.1103/physrevb.51.9302 · 1995 · External reference
Growth of unidirectional potassium dihydrogen orthophosphate single crystal by SR method and its characterization