Research graph
References from Prediction of creep deformation and rupture behaviour of 2.25Cr–1Mo weld joint. Local targets link to admitted publications; unresolved targets remain external evidence.
Remnant life assessment
1990 · External reference
The role of welding in component integrity
1990 · External reference
Diagram for the prediction of weld heat-affected zone microstructure
10.1179/030716977803292394 · 1977 · External reference
Unresolved reference
External reference
Unresolved reference
External reference
High temperature failure of thick-section, low alloy steel to stainless steel transition welds
10.1080/09603409.1994.11689467 · 1994 · External reference
Unresolved reference
1984 · External reference
Creep of butt-welded tubes
1981 · External reference
Geometrical effect on creep in cross weld specimens
10.1016/0308-0161(94)00009-8 · 1995 · External reference
Weld performance under creep using finite element modeling
10.1016/s0308-0161(97)00008-2 · 1997 · External reference
Extrapolation and creep life prediction for high temperature service
1984 · External reference
Unresolved reference
External reference
Unresolved reference
External reference
Unresolved reference
External reference
Unresolved reference
External reference
Unresolved reference
External reference
Creep behaviour of post-weld heat-treated 2.25Cr–1Mo ferritic steel base, weld metal and weldments
10.1016/0921-5093(90)90265-5 · 1990 · External reference
Temperature dependence of tensile properties of 2.25Cr–1Mo steel base, weldments simulated heat-affected zone structures
1993 · External reference
Creep deformation and local strain distributions in dissimilar metal welds between AISI type 316 and 2.25Cr–1Mo steels made with 17Cr–8Ni–2Mo weld metal
10.1179/030716984803274873 · 1984 · External reference
The tempering of 2 1/4%Cr–1%Mo steel after quenching and normalizing
1959 · External reference
Metallurgical changes in 2.25Cr–1Mo steels during creep-rupture test
1971 · External reference
The relative strengths of base metal and heat-affected zone in 2 1/4Cr–1Mo weldments — a microstructural evaluation
1986 · External reference
Unresolved reference
External reference
Precipitation sequence in heat affected zone of 2.25Cr–1Mo steel during stress-relief treatment
10.1179/030634581790426705 · 1981 · External reference
A creep rupture behaviour of weldments
1982 · External reference
Unresolved reference
External reference